5356 is about 5% Magnesium Aluminum filler metal which has high strength, high corrosion resistance and matches the color well with the parent metal after anodizing, recommended for welding casting and forging Al-Mg alloys with <5% Magnesium and parts of wrought alloy of 5000 series, 6000 series, 7000 series, such as 5050, 5052, 5083, 5456, 6005A, 6061,6063,6082,7005 etc.
POUŽÍVANÉ V SEKTORE TECHNOLÓGIE ŤAŽKÉHO PRIEMYSLU
ROKY SKÚSENOSTÍ S VÝSKUMOM A VÝVOJOM
DRUŽSTEVNÉ VEĽKÉ INŠTITÚCIE VÝSKUMU A VÝVOJA
KRAJINY A REGIÓNY GLOBÁLNEHO OBCHODU
Viac ako 90 % našich operátorov v teréne má odborné a technické vzdelanie a dlhoročné skúsenosti v oblasti spracovania a montáže zariadení. Práve vďaka tomuto zjednotenému, oddanému, priekopníckemu, kvalifikovanému a skúsenému tímu je možné technológie a produkty spoločnosti neustále aktualizovať a zlepšovať.
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Vidieť viac
Jul 29, 2026
Výber nesprávneho hliníkového plniaceho drôtu má tendenciu spôsobovať problémy dlho predtým, ako sa hotový diel dostane na nakladaciu...
Jul 27, 2026
Spojenie, ktoré sa zahrieva pri veľkej záťaži, kábel, ktorý sa po mesiacoch vibrácií stále uvoľňuje, drôt, ktorý po opakovanom ohýban...
Jul 22, 2026
Zvárač sa pripravuje na prácu hliníkom, zriedka prestane sa zistiť na koróziu až oveľa neskôr – zvyčajne vtedy, keď zavolá a spýta sa...
Jul 20, 2026
Výber nesprávneho hliníkového drôtu pre nastavenie MIG je jednou z tých chýb, ktoré sa prejavia neskoro, zvyčajne potom, čo je už zva...
Jul 29, 2026
Farebne zlaté zvary na eloxovanom hliníku sú notoricky ťažko postihnuteľné s prídavným kovom na všeobecné použitie, čo je presne t...
Jul 22, 2026
Výber nesprávneho plniaceho drôtu je jedným z najrýchlejších spôsobov, ako skončiť s prasknutými zvarmi, koroznymi poruchami alebo...
When working with aluminum alloys, selecting the right ER5356 aluminum welding wire can significantly impact weld quality, strength, and corrosion resistance. This versatile filler metal is particularly well-suited for MIG and TIG welding applications, especially when joining 5XXX series aluminum alloys commonly used in marine, automotive, and structural fabrication.
ER5356 stands out among aluminum welding wires due to its 5% magnesium content, which provides:
For welders working on boat hull repairs or aluminum trailer fabrication, ER5356 offers distinct advantages over other filler wires. Its compatibility with marine-grade aluminum alloys like 5052, 5083, and 5454 makes it a top choice for offshore welding projects.
When setting up for MIG welding aluminum with ER5356, proper equipment configuration is crucial:
Recommended Parameters:
To prevent common aluminum MIG welding problems like porosity or poor fusion:
For precision work on aluminum pipe welding or thin gauge aluminum fabrication, TIG welding with ER5356 produces clean, high-quality welds:
Optimal TIG Settings:
The anodizing compatibility of ER5356 makes it preferable for visible welds where a uniform finish is required, though it may show a slight gray tint compared to ER4043's darker appearance.
| Parameter | ER5356 | ER4043 |
|---|---|---|
| Tensile Strength | 290 MPa | 186 MPa |
| Elongation | 10-15% | 12-18% |
| Color After Anodizing | Light Gray | Dark Gray |
| Magnesium Content | 5% | 0% |
| Best Applications | Marine, Structural | Castings, Decorative |
| Corrosion Resistance | Excellent (saltwater) | Good |
| Weld Cracking Resistance | High | Moderate |